Shear heating phenomena during injection molding of rubber compounds greatly affect product quality but are difficult to control and replicate with laboratory tests. In this work, a very fast online process control of industrial injection molding is proposed, based on the measurement of surface temperature by infrared thermal camera of the rubber as it leaves the extruder barrel. Moreover, a new technological parameter (shear heating parameter, ηSH) is calculated from the measured temperature. A robust correlation between ηSH and viscosity from rheometric laboratory measurements was achieved for different rubber compounds. This represents an operating roadmap to support the process engineer in the improvement of process control. To show the potential of this tool, it was successfully used to optimize the injection molding of industrial production of AEM rubber compound affected by scorching and thermal degradation issues. ηSH was found to be suitable for industrial practice and able to provide accurate information about thermal history and process safety.
Applications of shear heating parameter for injection molding process optimization of AEM rubber compounds
Ramini M.
;Agnelli S.;Ramorino G.
2022-01-01
Abstract
Shear heating phenomena during injection molding of rubber compounds greatly affect product quality but are difficult to control and replicate with laboratory tests. In this work, a very fast online process control of industrial injection molding is proposed, based on the measurement of surface temperature by infrared thermal camera of the rubber as it leaves the extruder barrel. Moreover, a new technological parameter (shear heating parameter, ηSH) is calculated from the measured temperature. A robust correlation between ηSH and viscosity from rheometric laboratory measurements was achieved for different rubber compounds. This represents an operating roadmap to support the process engineer in the improvement of process control. To show the potential of this tool, it was successfully used to optimize the injection molding of industrial production of AEM rubber compound affected by scorching and thermal degradation issues. ηSH was found to be suitable for industrial practice and able to provide accurate information about thermal history and process safety.File | Dimensione | Formato | |
---|---|---|---|
EPL-0011569_article.pdf
accesso aperto
Descrizione: Full paper
Tipologia:
Full Text
Licenza:
Non specificato
Dimensione
4.62 MB
Formato
Adobe PDF
|
4.62 MB | Adobe PDF | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.