This study investigates the cavitation erosion resistance of AlSi10Mg additive manufactured samples according to the ASTM G32 standard, in comparison with the cast ones. Samples were tested in different conditions in order to analyse the effect of T6 heat treatment and hot isostatic pressing, while cast samples were studied in as-cast and heat-treated conditions. It was found that additive manufactured AlSi10Mg alloy shows outstanding cavitation erosion resistance, in comparison to the cast alloy, mainly due to the ultra-fine microstructure. This superior performance of as-produced AlSi10Mg additive manufactured samples was demonstrated by the extremely limited mass loss and erosion rate measured during the tests, coupled with a remarkably long incubation stage. On the other hand, the heat treatment proves detrimental to the cavitation resistance of additive manufactured material due to the microstructure modification and pores enlargement. Hot isostatic pressing only partially improves the alloy performance.

Investigation of cavitation erosion resistance of AlSi10Mg alloy for additive manufacturing

GIRELLI, LUCA
;
Tocci, Marialaura;Montesano, Lorenzo;Gelfi, Marcello;Pola, Annalisa
2018-01-01

Abstract

This study investigates the cavitation erosion resistance of AlSi10Mg additive manufactured samples according to the ASTM G32 standard, in comparison with the cast ones. Samples were tested in different conditions in order to analyse the effect of T6 heat treatment and hot isostatic pressing, while cast samples were studied in as-cast and heat-treated conditions. It was found that additive manufactured AlSi10Mg alloy shows outstanding cavitation erosion resistance, in comparison to the cast alloy, mainly due to the ultra-fine microstructure. This superior performance of as-produced AlSi10Mg additive manufactured samples was demonstrated by the extremely limited mass loss and erosion rate measured during the tests, coupled with a remarkably long incubation stage. On the other hand, the heat treatment proves detrimental to the cavitation resistance of additive manufactured material due to the microstructure modification and pores enlargement. Hot isostatic pressing only partially improves the alloy performance.
2018
Altre fonti
PE8_9 Materials engineering (biomaterials, metals, ceramics, polymers, composites,…)
Esperti anonimi
Inglese
Internazionale
ELETTRONICO
402-403
124
136
13
Cavitation erosion; Electron microscopy; Erosion testing; Non-ferrous metals; Optical microscopy; Condensed Matter Physics; Mechanics of Materials; Surfaces and Interfaces; Surfaces, Coatings and Films; Materials Chemistry2506 Metals and Alloys
no
5
info:eu-repo/semantics/article
262
Girelli, Luca; Tocci, Marialaura; Montesano, Lorenzo; Gelfi, Marcello; Pola, Annalisa
1 Contributo su Rivista::1.1 Articolo in rivista
none
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11379/501682
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 50
  • ???jsp.display-item.citation.isi??? 43
social impact