Alginate-TiO2 porous beads were investigated in adsorption and removal of different organic dyes from water. The beads were fabricated from commercial HOMBIKAT type II anatase powders through ionotropic gelation, using alginate as a non-toxic, biocompatible pore-directing template and binder. Both anionic (methyl orange, MO) and cationic (methylene blue, MB) dyes were utilized as a model of organic pollutants. The photocatalytic activity of titania in solution is slightly reduced if compared with that of the nanopowders before assembly. However, the formation of the beads brings along many direct advantages. Thanks to their large size (0.5-2 mm) and good mechanical stability, the beads can be easily dispersed in polluted solutions and promptly recovered when stirring is stopped. The beads exhibited a strongly enhanced adsorption of MB in comparison to nanopowder samples (55% vs. 6.5%). Upon recovery, the adsorbed dye can be completely extracted and removed from the beads either by UV or ozone -UV cleaner treatment. The latter procedure resulted in a further increment of adsorption efficiency (up to 64%) as a function of different adsorption-removal cycles.

Easy recovery, mechanical stability, enhanced adsorption capacity and recyclability of alginate-based TiO2 macrobead photocatalysts for water treatment

GJIPALAJ, Joana;ALESSANDRI, Ivano
2017-01-01

Abstract

Alginate-TiO2 porous beads were investigated in adsorption and removal of different organic dyes from water. The beads were fabricated from commercial HOMBIKAT type II anatase powders through ionotropic gelation, using alginate as a non-toxic, biocompatible pore-directing template and binder. Both anionic (methyl orange, MO) and cationic (methylene blue, MB) dyes were utilized as a model of organic pollutants. The photocatalytic activity of titania in solution is slightly reduced if compared with that of the nanopowders before assembly. However, the formation of the beads brings along many direct advantages. Thanks to their large size (0.5-2 mm) and good mechanical stability, the beads can be easily dispersed in polluted solutions and promptly recovered when stirring is stopped. The beads exhibited a strongly enhanced adsorption of MB in comparison to nanopowder samples (55% vs. 6.5%). Upon recovery, the adsorbed dye can be completely extracted and removed from the beads either by UV or ozone -UV cleaner treatment. The latter procedure resulted in a further increment of adsorption efficiency (up to 64%) as a function of different adsorption-removal cycles.
File in questo prodotto:
File Dimensione Formato  
Gjipalaj_JECE_2017.pdf

solo utenti autorizzati

Tipologia: Documento in Post-print
Licenza: PUBBLICO - Pubblico con Copyright
Dimensione 3.06 MB
Formato Adobe PDF
3.06 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11379/490818
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 55
  • ???jsp.display-item.citation.isi??? 45
social impact