Ultraviolet absorption and Circular Dichroism spectra in the region 300-700 nm for highly regioregular samples of Poly{3[(S)-2-methylbutyl]-thiophene} are reported for solutions in good and bad solvents, at variable temperature, and for films in various conditions. In the latter case novel CD data up to the melting temperature provide some hints for the self-assembling process towards supramolecular organization. UV and CD data are also reported on the related polymer Poly{3,4-di[(S)-2-methylbutyl]-thiophene}.

Circular Dichroism Spectra of Regioregular Poly[3[(S)-2-methylbutyl]-thiophene] and of Poly[3,4-di[(S)-2-methylbutyl]-thiophene]

LEBON, France;LONGHI, Giovanna;ABBATE, Sergio
;
2002-01-01

Abstract

Ultraviolet absorption and Circular Dichroism spectra in the region 300-700 nm for highly regioregular samples of Poly{3[(S)-2-methylbutyl]-thiophene} are reported for solutions in good and bad solvents, at variable temperature, and for films in various conditions. In the latter case novel CD data up to the melting temperature provide some hints for the self-assembling process towards supramolecular organization. UV and CD data are also reported on the related polymer Poly{3,4-di[(S)-2-methylbutyl]-thiophene}.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11379/21228
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? 0
  • Scopus 12
  • ???jsp.display-item.citation.isi??? 11
social impact